[1] National Bureau of Statistics of China. China Statistical Yearbook[M]. Beijing: China Statistics Press, 2011.(in Chinese)
中华人民共和国国家统计局.中国统计年鉴[M].北京:中国统计出版社,2011.
[2] LIU Wei, XING Feng, XIE You-jun. Influence of mineral admixture on the water sorptivity of concrete[J]. Journal of Shenzhen University Science and Engineering, 2008,25(3): 303-307.(in Chinese)
刘伟, 邢锋, 谢友均. 矿物掺合料对混凝土毛细吸水性的影响[J]. 深圳大学学报理工版,2008, 25(3): 303-307.
[3] ZHANG Xiu-zhi,SUN Wei,RONG Zhi-dan,et al.Influence of reactive mineral admixtures on microstructure of ultra-high performance cementitious composites[J]. Journal of Shenzhen University Science and Engineering. 2008,25(4): 338-334.(in Chinese)?
张秀芝, 孙伟, 戎志丹, 等. 活性矿物掺合料对超高性能水泥基材料的影响[J]. 深圳大学学报理工版. 2008, 25(4): 338-334.
[4] ZHU Gui-zhen. Study on incineration of hazardous waste with cement turning kiln[J]. Environmental Protection,2000, 3:14-16.(in Chinese)
朱桂珍.利用水泥回转窑焚烧处置危险废物的评价研究[J].环境保护,2000, 3:14-16.?
[5] Zhang J L, Liu J G, Li C, et al. Comparison of the fixation effects of heavy metals by cement rotary kiln co-processing and cement based solidification/stabilization[J]. Journal of Hazardous Materials, 2009, 165(1-3):1179-1185.
[6] Wang L, Jin Y Y, Nie Y F, et al. Recycling of municipal solid waste incineration fly ash for ordinary Portland cement production: a real-scale test[J]. Resources, Conservation and Recycling, 2010, 54(12): 1428-1435.
[7] Yang Y F, Yang Y, Wang Q H, et al. Release of heavy metals from concrete made with cement from cement kiln co-processing of hazardous wastes in pavement scenarios[J]. Environmental Engineering Science, 2011, 28(1): 35-42.?
[8] WANG Lei, JIN Yi-ying, NIE Yong-feng, et al. Stabilization of arsenic in waste during co-processing with cement kiln and leaching characteristics of clinker[J]. Huagong Xuebao, 2011, 62(3): 816-822.(in Chinese)
王雷, 金宜英, 聂永丰, 等. 废物水泥窑共处置过程砷的固定特性及产物的环境安全性[J]. 化工学报, 2011, 62(3): 816-822.
[9] WANG Lei, JIN Yi-ying, NIE Yong-feng,et al. Characteristics of arsenic migration in MSWI fly ash during co-processing with a cement kiln[J]. Acta Scientiae Circumstantiae, 2011, 31(2): 407-413.(in Chinese)
王雷, 金宜英, 聂永丰, 等. 焚烧飞灰水泥窑共处置过程As的迁移特征[J]. 环境科学学报, 2011, 31(2): 407-413.
[10] Yan D H,Karstensen K H,Huang Q F,et al.Coprocessing of industrial and hazardous wastes in cement kilns: a review of current status and future needs in China[J]. Environmental Engineering Science, 2010, 27(1): 37-45.
[11] LIU Han-qiao, WEI Guo-xia, LIANG Yin, et al. Effects of additive on crystallization behaviour of arc-molten slag from incinerator fly ash[J]. Journal of Shenzhen University Science and Engineering, 2011,28(6):559-564.(in Chinese)
刘汉桥, 魏国侠, 梁茵, 等. 配料对焚烧飞灰电弧炉熔渣晶化行为的影响[J]. 深圳大学学报理工版, 2011, 28(6): 559-564.
[12] Wang L, Jin Y Y, Nie Y F. Investigation of accelerated and natural carbonation of MSWI fly ash with a high content of Ca[J]. Journal of Hazardous Materials, 2010, 174(15): 334-343.
[13] Shi H S, Deng K, Yuan F, et al. Preparation of the saving-energy sulphoaluminate cement using MSWI fly ash[J]. Journal of Hazardous Materials, 2009, 169: 551-555.
[14] ZHANG Jun-li, LIU Jian-guo, LI Cheng, et al. Comparison of fixation effects of heavy metals between cement rotary kiln co-processing and cement solidification/stabilization[J]. Environmental Science, 2008,29(4):1138-1142.(in Chinese)
张俊丽,刘建国,李橙,等.水泥窑协同处置与水泥固化/稳定化对重金属的固定效果比较[J].环境科学, 2008,29(4):1138-1142.
[15] LI Cheng, LIU Jian-guo, ZHANG Jun-li, et al. Dynamic leaching behavior of heavy metals in eco-cement mortar block[J]. Environmental Science, 2008,29(3):831-836.(in Chinese)
李橙,刘建国,张俊丽,等.生态水泥胶砂块中重金属的动态浸出行为研究[J].环境科学,2008,29(3):831-836.
[16] CUI Su-ping, LAN Ming-zhang, ZHANG Jiang, et al. Effect and incorporation mechanism of heavy metal elements in hazardous industrial wastes during clinker formation[J]. Journal of the Chinese Ceramic Society,2004,32(10):1264-1270.(in Chinese)
崔素萍,兰明章,张江,等.废弃物中重金属元素在水泥熟料形成过程中的作用及其固化机理[J].硅酸盐学报, 2004,32(10):1264-1270.
[17] ZHU Gui-zhen. Study on using cement turning kiln to incinerate hazardous waste along with cement materials[J]. Acta Scientiae Circumstantiae,2000,20(6): 810-812.(in Chinese)
朱桂珍.利用水泥回转窑焚烧处置危险废物的评价研究[J].环境科学学报, 2000, 20(6):810-812.
[18] Guo Q Z. Increases of lead and chromium in drinking water from using cement-mortar-lined pipes: initial modeling and assessment[J]. Journal of Hazardous Materials, 1997, 56:18l-213.
[19] Guo Q Z, James O, Eckert J R. Heavy metal outputs from a cement kiln co-fired with hazardous waste fuels[J]. Journal of Hazardous Materials, 1996, 51: 47-65.