[1]刘汉桥,魏国侠,梁茵,等.配料对焚烧飞灰电弧炉熔渣晶化行为的影响[J].深圳大学学报理工版,2011,28(No.6(471-564)):559-564.
 LIU Han-qiao,WEI Guo-xia,LIANG Yin,et al.Effects of additive on crystallization behaviour of arc-molten slag from incinerator fly ash[J].Journal of Shenzhen University Science and Engineering,2011,28(No.6(471-564)):559-564.
点击复制

配料对焚烧飞灰电弧炉熔渣晶化行为的影响()
分享到:

《深圳大学学报理工版》[ISSN:1000-2618/CN:44-1401/N]

卷:
第28卷
期数:
2011年No.6(471-564)
页码:
559-564
栏目:
环境与能源
出版日期:
2011-11-20

文章信息/Info

Title:
Effects of additive on crystallization behaviour of arc-molten slag from incinerator fly ash
文章编号:
1000-2618(2011)06-0559-06
作者:
刘汉桥魏国侠梁茵杨俊兰
天津城市建设学院能源与机械工程系,天津 300384
Author(s):
LIU Han-qiaoWEI Guo-xiaLIANG Yinand YANG Jun-lan
Department of Energy and Mechanics Engineering, Tianjin Institute of Urban Construction, Tianjin 300384, P.R.China
关键词:
废物处理与综合利用垃圾焚烧飞灰废玻璃电弧炉熔融微晶玻璃
Keywords:
garbage processing and synthetical utilizationwaste incineration fly ashwaste glass culletelectronic arc-furnacemeltingglass-ceramics
分类号:
X 705
文献标志码:
A
摘要:
将垃圾焚烧飞灰电弧炉熔融处理后的液态熔渣直接浇铸成型后热处理,运用同步热分析仪、X射线衍射仪和扫描电镜等方法,研究废玻璃和晶核剂(TiO2和Cr2O3)等辅助原料的添加对微晶玻璃晶化行为及性能影响.研究表明,适量掺加废玻璃对微晶玻璃理化性能有显著改善,晶核剂类型及添加比对微晶玻璃主晶相和晶化程度影响较大,微晶玻璃的理想原料配比为m(废玻璃)∶m(垃圾焚烧飞灰)=1∶1,晶核剂TiO2添加质量分数为3%,制成的微晶玻璃主晶相为透辉石Ca(Mg,Al)(Si,Al)2O6和少量普通辉石Ca(Mg,Fe,Al)(Si,Al)2O6,抗弯强度54.96 MPa,主要理化性能达到或优于天然花岗岩和大理石,重金属浸出浓度低于国际建材环保要求限值.
Abstract:
To deal with the issue of municipal solid waste incineration fly ash,an ash melting treatment technology in combination with electric arc furnace metallurgical processes,was developed.The crystallization behavior of arc-melting slag form waste incineration fly ash was examined by differential thermal analysis (DTA),X-ray diffractometry(XRD), and scanning electron microscopy(SEM).Effects of additive waste glass cullet and nucleating agent on the crystallization behaviour,physical mechanical,and chemical characteristics were investigated.The results show that adding appropriate amount of waste glass will significantly improve the properties of glass-ceramics.The type and add ratio of nucleating agent have a greater impact on its crystallization behavior.The ideal raw material for glass formula is:mixed waste glass and waste incineration fly ash at 1∶1 ratio with nucleating agent of TiO2 added at 3%.The glass-ceramics with main crystalline phase of Ca(Mg,Al)(Si,Al)2O6 and Ca(Mg,Fe,Al)(Si,Al)2O6 has bending strength of 54.96 MPa.The physical mechanical and chemical characteristics are equivalent or superior to natural materials such as granite and marble.The leaching concentration of heavy metals is below environmentally regulatory thresholds of overseas building materials.

参考文献/References:

[1] 蔡九菊,刘汉桥,齐鹏飞,等.电弧炉熔融医疗垃圾焚烧灰的实验研究[J].过程工程学报,2007,7(2):337-341.
[2] 郭玉文,刘景洋,乔琦,等.TN型液晶焚烧产物及反应机理[J].深圳大学学报理工版,2010,27(1):76-81.
[3] Cheng T W,Tu C C,Ko M S,等.用小试和中试规模的等离子系统将焚烧灰制备微晶玻璃[J].国际陶瓷,2011,37(7):2437-2444.(英文版)
[4] HJ/T299-2007 固体废物浸出毒性浸出方法-硫酸硝酸法[S]
[5] Erol M,Kucukbayrak S,Mericboyu A E.粉煤灰制备的玻璃、微晶玻璃、陶瓷特性比较[J].危害物学报,2008,153(1):418-425.(英文版)
[6] Neda K,Vahak K M,Hamid R R,等.Al2O3含量对SiO2-Al2O3-CaO-MgO微晶玻璃晶化行为、微观结构和机械特性的影响[J].应用陶瓷技术国际期刊,2011,8(1):203-213.(英文版)
[7] 任祥忠,张培新,梁讯,等.MgO-Al2O3-SiO2系统微晶玻璃晶化行为研究[J].深圳大学学报理工版,2007,24(3):817-824.
[8] Barbieri L,Leonelli T,Manfreedini G,等.Cr2O3 对CaO-MgO-Al2O3-SiO2玻璃体系溶性、反应和成核作用的影响[J].危害物学报,1994,29(23):6273-6280.(英文版)
[9] GB5085.3-2007 危险废物鉴别标准 浸出毒性标准[S].
[10] Haugsten K,Gustavson B.有害和垃圾焚烧飞灰熔渣的环境特性[J],废物管理,2000,20(2/3):167-176.(英文版)
[11] 刘汉桥,魏国侠,梁茵.垃圾焚烧飞灰电弧炉熔渣制备微晶玻璃[J],中南大学学报,2011,18(6):1945-1952.(英文版)



[1] CAI Jiu-ju,LIU Han-qiao,QI Peng-fei,et al.Experimental study on melting of hospital waste incineration ash by electronic arc furnace[J].The Chinese Journal of Process Engineering,2007,7(2):337-341.(in Chinese)
[2] GUO Yu-wen,LIU Jing-yang,QIAO Qi,et al.Reaction mechanism of TN liquid crystal in incineration and its product assay[J].Journal of Shenzhen University Science and Engineering,2010,27(1):76-81.(in Chinese)
[3] Cheng T W,Tu C C,Ko M S,et al.Production of glass-ceramics from incinerator ash using lab-scale and pilot-scale thermal plasma systems[J].Ceramics International,2011,37(7):2437-2444
[4] HJ/T299-2007 Solid waste-extraction procedure for leaching toxicity-sulphuric acid & nitric acid method[S].(in Chinese)
[5] Erol M,Kucukbayrak S,Mericboyu A E.Comparison of the properties of glass,glass-ceramic and ceramic materials produced from coal fly ash[J].Journal of Hazardous Materials,2008,153(1):418-425.
[6] Neda K,Vahak K M,Hamid R R,et al.Effect of Al2O3 content on crystallization behavior,microstructure,and mechanical properties of SiO2-Al2O3-CaO-MgO glass-ceramics[J].International Journal of Applied Ceramic Technology,2011,8(1):203-213.
[7] REN Xiang-zhong ,ZHANG Pei-xin ,LIANG Xun,et al.Crystallization behaviors of MgO-Al2O3-SiO2 glass-ceramics[J].Journal of Shenzhen University Science and Engineering,2007,24(3):817-824.(in Chinese)
[8] Barbieri L,Leonelli T,Manfreedini G,et al.Solubility,reactivity and nucleation effect of Cr2O3 in the CaO-MgO-Al2O3-SiO2 glassy system[J].Journal of Hazardous Materials,1994,29(23):6273-6280.
[9] GB 5085.3-2007 Identification standard for hazardous wastes-identification for extraction procedure toxicity [S].(in Chinese)
[10] Haugsten K,Gustavson B.Environmental properties of vitrified fly ash from hazardous and municipal waste incineration[J]. Waste Management,2000,20(2/3):167-176.
[11] LIU Han-qiao,WEI Guo-xia,LIANG Yin,et al.Glass-ceramics made from arc-melting slag of waste incineration fly ash[J].Journal of Central South University of Technology,2011,18(6):1945-1952.

备注/Memo

备注/Memo:
收稿日期:2010-12-30;修回日期:2011-07-11
基金项目:国家自然科学基金青年科学基金资助项目(20806051);中国博士后科学基金资助项目(20080440680)
作者简介:刘汉桥(1973-),男(汉族),湖北省鄂州市人,天津城市建设学院副教授、博士.E-mail:lhqlkx@yahoo.com.cn
更新日期/Last Update: 2011-11-22